Secant Modulus 4.20 GPa

@Strain 0.500 %,
Temperature -40.0 °C
609 ksi

@Strain 0.500 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s..
Secant Modulus 4.20 GPa

@Strain 0.476 %,
Temperature -40.0 °C
609 ksi

@Strain 0.476 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider..
Secant Modulus 4.20 GPa

@Strain 0.500 %,
Temperature -40.0 °C
609 ksi

@Strain 0.500 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo..