Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 4.25 GPa @Strain 1.50 %, Temperature 80.0 °C |
616 ksi @Strain 1.50 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7.. |
|||
Secant Modulus | 4.25 GPa @Strain 0.400 %, Temperature 100 °C |
616 ksi @Strain 0.400 %, Temperature 212 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**) 33% Glass Reinforced UV Stabilized Polyamide 66 + Polyamide 6 Zytel 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provi.. |