Mechanical Properties Metric English Comments
Secant Modulus 2.79 GPa

@Strain 1.80 %,
Temperature 40.0 °C
405 ksi

@Strain 1.80 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov..
Secant Modulus 2.79 GPa

@Strain 2.08034 %,
Temperature 100 °C
405 ksi

@Strain 2.08034 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti..