Secant Modulus 2.84 GPa

@Strain 1.50 %,
Temperature 100 °C
412 ksi

@Strain 1.50 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8..