Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 3.35 GPa @Strain 1.10 %, Temperature -40.0 °C |
487 ksi @Strain 1.10 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized High Viscosity Polyamide 66 Zytel E51HSB NC010 is a high molecular weight heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by .. |
|||
Secant Modulus | 3.35 GPa @Strain 2.83 %, Temperature -40.0 °C |
487 ksi @Strain 2.83 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 132F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 132F NC010 is a nucleated lubricated polyamide 66 for injection molding. It was developed for fast production cycles and high productivity applications.Info.. |