Mechanical Properties Metric English Comments
Secant Modulus 3.43 GPa

@Strain 2.06534 %,
Temperature 40.0 °C
497 ksi

@Strain 2.06534 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK612SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
15% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK612SF is a 15% glass fiber reinforced low viscosity polybutylene terephthalate for injecti..