Polymer Property : Secant Modulus = 5.18 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 5.18 GPa

@Strain 1.50 %,
Temperature 40.0 °C
751 ksi

@Strain 1.50 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8..
Secant Modulus 5.18 GPa

@Strain 2.11 %,
Temperature 80.0 °C
751 ksi

@Strain 2.11 %,
Temperature 176 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FR52G30NH NC010 Polyphthalamide (PPA)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It..