Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 5.4921 GPa @Strain 0.100 %, Temperature 100 °C |
796.57 ksi @Strain 0.100 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT) 30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on pol.. |
|||
Secant Modulus | 5.4921 GPa @Strain 0.100 %, Temperature 100 °C |
796.57 ksi @Strain 0.100 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3030G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with goo.. |