Polymer Property : Secant Modulus = 529 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 3.64 GPa

@Strain 0.450 %,
Temperature 40.0 °C
529 ksi

@Strain 0.450 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov..
Secant Modulus 3.65 GPa

@Strain 1.00 %,
Temperature -40.0 °C
529 ksi

@Strain 1.00 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical ..