Mechanical Properties Metric English Comments
Secant Modulus 3.71 GPa

@Strain 0.900 %,
Temperature -40.0 °C
538 ksi

@Strain 0.900 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500P BK602 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Improved ProcessingDelrin 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin 500P has improved pro..
Secant Modulus 3.71 GPa

@Strain 1.30 %,
Temperature 100 °C
538 ksi

@Strain 1.30 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on pol..
Secant Modulus 3.71 GPa

@Strain 1.30 %,
Temperature 100 °C
538 ksi

@Strain 1.30 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3030G NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with goo..