Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 6.00 GPa @Strain 0.250 %, Temperature 0.000 °C |
870 ksi @Strain 0.250 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT) 10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers |
|||
Secant Modulus | 6.00 GPa @Strain 1.70 %, Temperature -40.0 °C |
870 ksi @Strain 1.70 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3015G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 15% Glass Reinforced Polytrimethylene Terephthalate with Resin Made from Bio-PDO Sorona 3015G NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% ba.. |