Polymer Property : Secant Modulus = 6.68 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 6.68 GPa

@Strain 0.120 %,
Temperature 100 °C
969 ksi

@Strain 0.120 %,
Temperature 212 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FR52G30NH BK337 Polyphthalamide (PPA)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It..