Secant Modulus 0.419 GPa

@Strain 13.9 %,
Temperature 0.000 °C
60.8 ksi

@Strain 13.9 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 520MP NC010 Acetal (POM)  (Unverified Data**)
20% Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 520MP is a medium viscosity acetal homopolymer containing 20% Teflon PTFE Micropowder. It is designe..