Mechanical Properties Metric English Comments
Secant Modulus 0.43495 GPa

@Strain 7.01 %,
Temperature 40.0 °C
63.085 ksi

@Strain 7.01 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers
Secant Modulus 0.43495 GPa

@Strain 7.01 %,
Temperature 40.0 °C
63.085 ksi

@Strain 7.01 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for ..