Polymer Property : Secant Modulus = 72.5 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 0.500 GPa

@Strain 7.00 %,
Temperature 80.0 °C
72.5 ksi

@Strain 7.00 %,
Temperature 176 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500P BK602 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Improved ProcessingDelrin 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin 500P has improved pro..