Mechanical Properties Metric English Comments
Secant Modulus 0.548 GPa

@Strain 6.00 %,
Temperature 80.0 °C
79.5 ksi

@Strain 6.00 %,
Temperature 176 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 11C40 NC010 Nylon 66  (Unverified Data**)
40% Mineral Reinforced Polyamide 66 Minlon 11C40 NC010 is a 40% mineral reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers