Mechanical Properties Metric English Comments
Secant Modulus 0.575 GPa

@Strain 4.80 %,
Temperature 100 °C
83.4 ksi

@Strain 4.80 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s..
Secant Modulus 0.575 GPa

@Strain 4.80 %,
Temperature 100 °C
83.4 ksi

@Strain 4.80 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo..