Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.637 GPa @Strain 6.00 %, Temperature 80.0 °C |
92.3 ksi @Strain 6.00 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
Secant Modulus | 0.637 GPa @Strain 6.00 %, Temperature 80.0 °C |
92.3 ksi @Strain 6.00 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo.. |