Secant Modulus 6.80 GPa

@Strain 0.250 %,
Temperature -40.0 °C
986 ksi

@Strain 0.250 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT)