Mechanical Properties Metric English Comments
Puncture Energy 1.60 J

@Thickness 2.50 mm,
Temperature -40.0 °C
1.18 ft-lb

@Thickness 0.0984 in,
Temperature -40.0 °F
max load; ASTM D3763
Eastman 9921 PET Injection Molded  (discontinued **)
VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p..
Puncture Energy 1.60 J

@Temperature 23.0 °C
1.18 ft-lb

@Temperature 73.4 °F
Energy @ Max. Load; ASTM D3763
Eastman Cadence™ GS1 Copolyester for film calendering
Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe..
Puncture Energy 1.60 J

@Thickness 2.50 mm,
Temperature -40.0 °C
1.18 ft-lb

@Thickness 0.0984 in,
Temperature -40.0 °F
max load; ASTM D3763
Eastman Eastar EN001 Copolyester
Eastar EN001 Copolyester is a thermoplastic polyester copolymer. Eastar EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming pro..
Puncture Energy 1.60 J

@Thickness 2.50 mm,
Temperature -40.0 °C
1.18 ft-lb

@Thickness 0.0984 in,
Temperature -40.0 °F
max load; ASTM D3763
Eastman Eastar MN021 Copolyester
Eastar copolyester MN021 is a thermoplastic condensation copolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz..
Puncture Energy 1.60 J

@Thickness 2.50 mm,
Temperature -40.0 °C
1.18 ft-lb

@Thickness 0.0984 in,
Temperature -40.0 °F
max load; ASTM D3763
Eastman 9921W PET Injection Molded  (discontinued **)
Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters ..