Polymer Property : Puncture Energy = 14.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 14.0 J

@Temperature 23.0 °C
10.3 ft-lb

@Temperature 73.4 °F
cond.; ISO 6603-2
Lanxess Durethan® BKV 50 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 50% glass fibers, injection moldingInformation provided by LANXESS.