Polymer Property : Puncture Energy = 160 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 160 J

@Temperature 23.0 °C
118 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Lanxess Durethan® B 40 SK 000000 Nylon 6
PA 6, non-reinforced, injection molding
Puncture Energy 160 J

@Temperature -30.0 °C
118 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® B 40 SK 000000 Nylon 6
PA 6, non-reinforced, injection molding