Mechanical Properties Metric English Comments
Puncture Energy 28.0 J

@Thickness 2.50 mm,
Temperature 23.0 °C
20.7 ft-lb

@Thickness 0.0984 in,
Temperature 73.4 °F
max load; ASTM D3763
Eastman Drystar 0601 Copolyester, Injection Molded
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
Puncture Energy 28.0 J

@Thickness 2.50 mm,
Temperature 23.0 °C
20.7 ft-lb

@Thickness 0.0984 in,
Temperature 73.4 °F
At Max load; ASTM D3763
Eastman Eastman 1223 Copolyester
Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card..