Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 38.0 J @Temperature 23.0 °C |
28.0 ft-lb @Temperature 73.4 °F |
At Max load; ASTM D3763 |
Eastman Aspira EN177 Copolyester Resin for Extrusion Blow Molding Applications:Beverage packagingConsumer packagingFood packagingPersonal care packagingKey Attributes:BPA-freeCompatible with high-output manufacturing platformsExcellent clarityHigh gloss appearance.. |
|||
Puncture Energy | 38.0 J @Temperature 23.0 °C |
28.0 ft-lb @Temperature 73.4 °F |
At Max load; ASTM D3763 |
Eastman Provista NXT Copolymer Resin for Profile Extrusion Applications:Candy packagingCorner guardsDisplays, Fixtures and Point of purchaseFood packagingFurniture guardsIntegrated circuit tubesLighting tubesPlastics for hygiene feminine productsPricing cha.. |
|||
Puncture Energy | 38.0 J @Temperature -40.0 °C |
28.0 ft-lb @Temperature -40.0 °F |
At Max load; ASTM D3763 |
Eastman Eastar EN059 Copolyester, Natural Applications:Cosmetics/personal care packagingDeodorant PackagingFragrance packagingOral hygienePlastics for hygiene feminine productsToothbrushesToys/Sporting goodsWriting instrumentsProduct Descri.. |