Polymer Property : Puncture Energy = 31.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 42.0 J

@Temperature 0.000 °C
31.0 ft-lb

@Temperature 32.0 °F
At Max load; ASTM D3763
Eastman Spectar® Clear Copolyester for Thermoforming
Applications:Decorative Light-Transmitting PanelsHeavy gauge sheet displaysKey Attributes:Easy to print and decorateExcellent clarityExcellent thermoforming characteristicsGood chemical resistanceOd..