Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 45.0 J @Temperature 23.0 °C |
33.2 ft-lb @Temperature 73.4 °F |
At Max load; ASTM D3763 |
Eastman DuraStar MN620 Polymer, Natural Applications:Blood therapyDrug deliveryIV componentsMedicalSurgical instrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAProduct Description: DuraStar Poly.. |
|||
Puncture Energy | 45.0 J @Temperature 23.0 °C |
33.2 ft-lb @Temperature 73.4 °F |
ISO 6603-2 |
Covestro Bayblend® W85 HI PC ASA Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Imp.. |
|||
Puncture Energy | 45.0 J @Temperature -30.0 °C |
33.2 ft-lb @Temperature -22.0 °F |
ISO 6603-2 |
Covestro Bayblend® W85 HI PC ASA Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Imp.. |
|||
Puncture Energy | 45.0 J @Temperature 23.0 °C |
33.2 ft-lb @Temperature 73.4 °F |
ISO 6603-2 |
Covestro Makrolon® 6255 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Lo.. |