Mechanical Properties Metric English Comments
Puncture Energy 66.0 J

@Temperature -40.0 °C
48.7 ft-lb

@Temperature -40.0 °F
Energy @ Max. Load; ASTM D3763
Eastman Tritan MX710 Copolyester
Eastman Tritan Copolyester MX710 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX710 has many outstanding features that include excellent toughness, hydr..
Puncture Energy 66.0 J

@Temperature -40.0 °C
48.7 ft-lb

@Temperature -40.0 °F
Energy @ Max. Load; ASTM D3763
Eastman Tritan MX711 Copolyester
Eastman Tritan Copolyester MX711 is an amorphous product with excellent appearance and clarity. Eastman Tritan MX711 contains a mold release derived from vegetable based sources. Eastman Tritan Co..