Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Resistance | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 180 |
Solvay Technyl® C 206 Nylon 6, EH0 Unreinforced Plyamide PA6, standard for fast cycling, for injection molding.Technyl C 206 has high fluidity and good mold release, favored by a high crystallization rate. It is specially suitable f.. |