Polymer Property : Izod Impact Resistance = 0.809 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Resistance 0.170 J/cm²

@Temperature 23.0 °C
0.809 ft-lb/in²

@Temperature 73.4 °F
ISO 180
LyondellBasell Astryn BR33GC Polypropylene Copolymer, Mineral Filled
Key Features: conventional melt flow, high modulus, UV-stabilized, mineral-filled polypropylene copolymer, high rigidity, high impact strength, good dimensional stability, low foggingApplications: k..