Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Resistance | 1.40 J/cm² | 6.66 ft-lb/in² | ISO 180 |
Solvay Technyl® C 216 Nylon 6, 30% Glass Fiber, EH0 Polyamide PA6, reinforced with 30% of glass fiber, for injection molding.It has good mechanical properties. It is used in all sectors of industry, offering an excellent combination between thermal .. |
|||
Izod Impact Resistance | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 180/1A |
DSM Stanyl® TW271F8 (PA46+PTFE)-GF40 40% Glass Reinforced, Heat Stabilized, Wear and Friction Modified |