Polymer Property : Izod Impact Resistance = 13.8 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Resistance 2.90 J/cm²
13.8 ft-lb/in²
Dow DOWLEX™ IP-42 High Density Polyethylene
DOWLEX® IP-42 resin is an improved processing high density polyethylene resin designed for excellent flow and high impact. DOWLEX IP-42 resin is designed by optimizing the breadth and shape of the ..