Mechanical Properties Metric English Comments
Izod Impact Resistance 3.20 J/cm²
15.2 ft-lb/in²
ASTM D256
Zhejiang Double Fish YS-G050 50% Long Fiber Glass Reinforced Polypropylene
Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm..
Izod Impact Resistance 3.20 J/cm²
15.2 ft-lb/in²
Dow HDPE 30460M High Density Polyethylene
DOW HDPE 30460M resin is a medium molecular weight distribution copolymer designed to offer moderate impact strength and stress crack resistance with excellent rigidity. This resin has excellent pro..