Mechanical Properties Metric English Comments
Izod Impact Resistance 8.50 J/cm²
40.5 ft-lb/in²
Denka TH-21 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..