Polymer Property : Izod Impact Resistance = 5.24 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Resistance 1.10 J/cm²
5.24 ft-lb/in²
ISO 180
Solvay Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH0
Polyamide PA66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V30 is used in all sectors of industry, offering an excellent combination between thermal and..
Izod Impact Resistance 1.10 J/cm²
5.24 ft-lb/in²
ISO 180
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH0
Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope..
Izod Impact Resistance 1.10 J/cm²
5.24 ft-lb/in²
Dow DOWLEX™ IP-90 High Density Polyethylene
Next Generation DOWLEX® IP-90 resin is a high flow improved processing high density polyethylene resin designed for ultra-thin wall injection molded containers and drink cups. This resin has been m..