Polymer Property : Izod Impact Resistance = 6.00 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Resistance 6.00 J/cm²
28.6 ft-lb/in²
ISO 180
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH0
Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin..