Polymer Property : Dynatup @ -18°C = 31.7 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dynatup @ -18°C 43.0 J
31.7 ft-lb
Energy at Maximum Load. Dry as molded. 23°C; D3763
Solvay Specialty Polymers Amodel® ET-1001 L Polyphthalamide (PPA) Resin, Dry as Molded  (discontinued **)
AMODEL ET-1001 L resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resistan..