Polymer Property : Heat Seal Strength, Ultimate = 14.7 N Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Heat Seal Strength, Ultimate 14.7 N
3.30 lb (f)
at 160°C, 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
Dow TUFLIN™ HS-7094 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Good Processability at Narrow Die Gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a TUFLIN™ HS-7094 NT 7 is a fractional melt, ethylene-hexene copolymer, designe..