Polymer Property : Film Tensile Strength at Break, MD = 13100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 90.0 MPa

@Thickness 0.100 mm
13100 psi

@Thickness 0.00394 in
ISO 527
Victrex® APTIV® 2102-100M Polyetheretherketone (PEEK) Polymer Film, Amorphous, Mineral Filled
APTIV® 2100 series films are the mineral filled amorphous films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications. APTIV ..