Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 16.5 MPa @Temperature 100 °C |
2400 psi @Temperature 212 °F |
|
DuPont™ Tedlar® SP TTRJ10SH9 Clear Polyvinyl Fluoride Film Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistance, and ease of cleaning ex.. |