Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 80.0 MPa @Thickness 0.125 mm |
11600 psi @Thickness 0.00492 in |
ISO 527 |
Victrex® APTIV® 2102-100M Polyetheretherketone (PEEK) Polymer Film, Amorphous, Mineral Filled APTIV® 2100 series films are the mineral filled amorphous films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications. APTIV .. |