Mechanical Properties | Metric | English | Comments |
---|---|---|---|
200% Modulus | 0.00250 GPa | 0.363 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Aerosil 200 Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
200% Modulus | 0.00250 GPa | 0.362 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Oyster Shell Calcium Carbonate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
200% Modulus | 0.00250 GPa | 0.363 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 30 PHR Fumed Silica - Wacker HK N20 MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
200% Modulus | 0.00250 GPa | 0.363 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Aerosil 200 Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
200% Modulus | 0.00250 GPa | 0.362 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Non-Black, Oyster Shell Calcium Carbonate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
200% Modulus | 0.00250 GPa | 0.363 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 30 PHR Fumed Silica - Wacker HK N20 MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |