Mechanical Properties Metric English Comments
200% Modulus 0.00315 GPa
0.457 ksi
10 in/min; ASTM D412
PolyOne Elastamax XL 1092-2 TPU-Based Thermoplastic Elastomer  (discontinued **)
This is a general purpose thermoplastic elastomer based on modified TPU technology. Physical Form: Pellet. Standard Color: Natural.Information provided by M. A. Hanna. M. A. Hanna and Geon merged..