Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 200% Modulus = 0.00360 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
200% Modulus 0.00360 GPa
0.522 ksi
ASTM D412; ASTM D638
Lubrizol Estane® 58252 Thermoplastic Polyurethane
Type: Estane® 58252 is a 70A polyether-type thermoplastic polyurethane (TPU).Features: Formulated to have one of the highest MVT values within the thermoplastic polyurethane class. It is also amon..
Copyright © lookpolymers.com All Rights Reserved