Polymer Property : 200% Modulus = 0.01231 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
200% Modulus 0.01231 GPa
1.785 ksi
TSE Industries Millathane® 66 Millable Polyurethane Rubber
Millathane 66 is a peroxide-curable polyurethane rubber for the production of oil, fuel and chemical resistant parts which require excellent low and high temperature performance and high mechanical ..
200% Modulus 0.01231 GPa
1.785 ksi
TSE Industries Millathane® 66 Millable Polyurethane Rubber
Millathane 66 is a peroxide-curable polyurethane rubber for the production of oil, fuel and chemical resistant parts which require excellent low and high temperature performance and high mechanical ..