Mechanical Properties | Metric | English | Comments |
---|---|---|---|
200% Modulus | 0.00490 GPa | 0.711 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR MBT MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
200% Modulus | 0.00490 GPa | 0.711 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR MBT MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |