Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 200% Modulus = 0.870 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
200% Modulus 0.00600 GPa
0.870 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR Thanecure ZM
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
200% Modulus 0.00600 GPa
0.870 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR Thanecure ZM
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
200% Modulus 0.00600 GPa
0.870 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 5.0 PHR Di-Cup 40C
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
200% Modulus 0.00600 GPa
0.870 ksi
ISO 37
AlphaGary Evoprene™ HP 3732 High Performance Thermoplastic Elastomer
Evoprene™ HP is a hydrogenated styrene block copolymer based thermoplastic elastomer. Specially formulated for applications requiring high strength and excellent abrasion resistance, Evoprene™ HP..
200% Modulus 0.00600 GPa
0.870 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 5.0 PHR Di-Cup 40C
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..