Mechanical Properties | Metric | English | Comments |
---|---|---|---|
200% Modulus | 0.00793 GPa | 1.15 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
200% Modulus | 0.00793 GPa | 1.15 ksi | heat aged one week at 300ºF |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 60 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
200% Modulus | 0.00793 GPa | 1.15 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
200% Modulus | 0.00793 GPa | 1.15 ksi | heat aged one week at 300ºF |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 60 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |