Mechanical Properties | Metric | English | Comments |
---|---|---|---|
200% Modulus | 0.00841 GPa | 1.22 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 4.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
200% Modulus | 0.00841 GPa | 1.22 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 4.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
200% Modulus | 0.00840 GPa | 1.22 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4725P Heat Resistant Molding FormulationNordel® IP 4725P |