Mechanical Properties | Metric | English | Comments |
---|---|---|---|
200% Modulus | 0.0207 GPa | 3.00 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 60 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
200% Modulus | 0.0207 GPa | 3.00 ksi | ASTM D412 |
Lubrizol Estane® ALR E60D Thermoplastic Polyurethane Type: Estane® ALR E60D is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corpor.. |
|||
200% Modulus | 0.0207 GPa | 3.00 ksi | ASTM D412 |
Lubrizol Estane® ALR E95A Thermoplastic Polyurethane Type: Estane® ALR E95A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corpor.. |
|||
200% Modulus | 0.0207 GPa | 3.00 ksi | |