Dart Drop Total Energy 20.0 - 55.0 J/cm

@Temperature -20.0 - 0.000 °C
0.0375 - 0.103 ft-lb/mil

@Temperature -4.00 - 32.0 °F
Average value: 37.5 J/cm Grade Count:1
Overview of materials for Polypropylene, Sheet/Thermoforming Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum..